Polyester yarn 111 tex*2 + cotton yarn 50 tex*61) Linear Density: 534,1 tex2) Relative deviation of conditioned linear density from rated: -1.1%3) Breaking weight (tensile strength): 17 kgs4) Elongation at break: 14.85) Terns per meter 1576) Laboratory humidity 3.95Polyester yarn: 43 %Cotton yarn: 57%Application: Yarn for rubber hose braidingP